Chandran, Gopi R and Patil, KC (1992) A rapid method to prepare crystalline fine particle chromite powders. In: Materials Letters, 12 (6). pp. 437-441.
PDF
A_rapid_Aug15th.pdf Restricted to Registered users only Download (613kB) | Request a copy |
Abstract
Fine particle $MgCr_2O_4, ZnCr_2O_4$ and $LaCrO_3$, have been obtained by rapidly heating an aqueous solution containing the corresponding metal (M) nitrate, chromium nitrate and maleie hydrazide in appropriate mole ratios at 375°C. The solution boils, froths and ignites to burn with a frame and yields voluminous chromite powders. Formation of spine1 chromites, $MCr_2O_4$, and pcrovskite $LaCrO_3$ was confirmed by their characteristic powder X-ray diffraction patterns and infrared spectra. The surface area of the chromites ranged from 32 to $72 m^{2/g}$.
Item Type: | Journal Article |
---|---|
Publication: | Materials Letters |
Publisher: | Elsevier |
Additional Information: | Copyright of this article belongs to Elsevier. |
Department/Centre: | Division of Chemical Sciences > Inorganic & Physical Chemistry |
Date Deposited: | 31 Oct 2006 |
Last Modified: | 19 Sep 2010 04:31 |
URI: | http://eprints.iisc.ac.in/id/eprint/8342 |
Actions (login required)
View Item |